• Product details image
16Cr25Ni20Si2 Heat-Resistant Stainless Steel
  • GB/T 1221
  • China
  • Stock
  • 16Cr25Ni20Si2

16Cr25Ni20Si2 heat-resistant stainless steel 16Cr25Ni20Si2 heat-resistant stainless steel has high high-temperature strength and oxidation resistance, and is more sensitive to sulfur-containing atmospheres. It has a tendency to embrittlemen

16Cr25Ni20Si2 Heat-Resistant Stainless Steel

16Cr25Ni20Si2 heat-resistant stainless steel
16Cr25Ni20Si2 heat-resistant stainless steel has high high-temperature strength and oxidation resistance, and is more sensitive to sulfur-containing atmospheres. It has a tendency to embrittlement of precipitated phases at 600-800 ℃. It is suitable for making various furnace components under stress.
 
Standard: GB/T 1221-2007
Grade: 16Cr25Ni20Si2

 
Equivalent grade
GB ISC ISO DIN EN/DIN NF EN/NF EN GOST BS EN/BS
16Cr25Ni20Si2 
(1Cr25Ni20Si2)
S38340 X15CrNiSi 25-21 X15CrNiSi 25-20 Z15CNS 25-20 X15CrNiSi 25-21 20Х25Н20С2 310S24

 
Chemical composition
Chemical composition C Si Mn P S Cr Ni
Min - 1.5 - - - 24 18
Max 0.2 2.5 1.5 0.045 0.03 27 21

 
Physical properties
Grade Physical properties
Tensile strength(MPa) Yield strength(MPa) Elongation(%) Reduction of area(%) Hardness
16Cr25Ni20Si2 ≥590 ≥295 ≥35 ≥50 ≤187HB
 
 
Heat treatment
Heat treatment specification: solid solution 1080~1130℃ fast cooling.
Metallographic structure: The structure is characterized by austenite.
 
 
Delivery status
Generally, the products are delivered in a heat-treated standard state, and the type of heat treatment is specified in the contract; if it is not specified, the goods are delivered in a non-heat-treated state.
 

Product key description, this is a very good product description, detailing our product use, product characteristics

Mail consultation
Please feel free to give your inquiry in the form below.We will reply you in 24 hours.